Figure 11 Sample from the turned section of the finial, average surface thickness 0.3 microns. (Photo, Winterthur Museum.) The surface history of this component contrasts with the flame but is similar to that of the replaced cartouche (figs. 9, 10). It may have been added at the same time as the cartouche.